Skip to main content

Nanoindentation, high-angular resolution electron backscatter diffraction (HR-EBSD), and transmission electron microscopy data in synthetic forsterite bicrystal samples (NERC Grant NE/S00162X/1)

Publisher
British Geological Survey (BGS)
Updated
2 October 2026
Topic
Not set
Licence
Not set

Summary

The data are nanoindentation, high-angular resolution electron backscatter diffraction (HR-EBSD), and transmission electron microscopy data collected on samples of synthetic forsterite bicrystals at room temperature. The data were collected in two samples, with high- and low- angle grain boundaries (HAGB, 60°, [100]/(011) and SB, 13°, [100]/(016)). The EBSD data are the basis for the HR-EBSD calculation. The HR-EBSD results are presented as Matlab data files. The nanoindentation data are categorised as a function of sample (‘ol13’ – low-angle grain boundary; and ‘ol60’ – high-angle grain boundary), and indenter tip geometry (spherical (with a 10 or 5 micron radius) and pyramidal (Berkovich). The data are presented in .xls files. The TEM data are presented as .tif files. The TEM data were collected in specific indents with various distances from the interfaces. These data have been published in the manuscript: : The Role of Grain Boundaries in Low-Temperature Plasticity of Olivine Revealed by Nanoindentation, with the DOI: 10.1029/2023JB026763

Data links

Link Format Preview Updated
Data – 2/10/2026

Is this data useful? Give us feedback

Additional information

Source Metadata
XML, HTML
Date added
02 October 2026
Harvest GUID
0bc51c9d-10cb-58ac-e063-0937940ae41d
Dataset reference date (creation)
2023-11-03
Frequency of update
notApplicable
Access constraints
The copyright of materials derived from the British Geological Survey's work is vested in the Natural Environment Research Council [NERC]. No part of this work may be reproduced or transmitted in any form or by any means, or stored in a retrieval system of any nature, without the prior permission of the copyright holder, via the BGS Intellectual Property Rights Manager. Use by customers of information provided by the BGS, is at the customer's own risk. In view of the disparate sources of information at BGS's disposal, including such material donated to BGS, that BGS accepts in good faith as being accurate, the Natural Environment Research Council (NERC) gives no warranty, expressed or implied, as to the quality or accuracy of the information supplied, or to the information's suitability for any use. NERC/BGS accepts no liability whatever in respect of loss, damage, injury or other occurence however caused.
Responsible party
University of Oxford (pointOfContact, originator); British Geological Survey (distributor, owner, pointOfContact)
ISO 19139 resource type